The sanding sequence, the raking-light inspection and the reference panel that decide how a restaurant chair looks under a dining room light.
Three grits, two inspections, one finish
Sanding is where a restaurant chair earns its surface. Three grits in sequence, an inspection under raking light between the second and third, and no finish until the bench signs off.
Finishes are specified for cleaning, not for depth of sheen. A restaurant seat is wiped with an alkaline agent several times a day, so the coating is chosen for chemical resistance, and the seat edges where the cloth catches are the first thing inspected.
Why sanding is compressed when a line is late
It is the easiest stage to rush and the first one the customer sees. A stain over a poorly sanded rail shows every scratch under a dining room light, so the schedule protects this bench, not the other way round.
Contract sections run heavier than domestic: 45 to 55 mm legs, 25 to 30 mm rails, and a stretcher on the models that get dragged rather than lifted. The extra section is not for show — it is what survives a room being re-set several times a day.
| Stage | Purpose | Check |
|---|---|---|
| Grit 1 | Flatten and shape | Machine marks gone |
| Grit 2 | Uniform scratch | Raking-light inspection |
| Grit 3 | Finish preparation | Bench sign-off |
| Stain / sealer | Colour vs reference panel | Under D65 light |
| Top coats | Scuff + tack between | Gloss and feel |
Sanding sequence
Species sand differently
Open-grain timber drinks stain and shows swirl marks; tight grain shows gloss differences. Grit sequence and sanding direction are set per species, not per shift.
Ash carries most of this programme and rubberwood covers the rest, both bought to a specification that assumes contract service: ash where the frame takes a daily racking load, rubberwood where the price point has to work.
Between coats, not just before them
Each finish coat gets a scuff and a tack cloth before the next; the final coat is compared against a sealed reference panel, not against the piece next to it.
EN 16139 Level 2 is the contract grade: higher cycle counts on seat and back, a leg forward load, and a stability test that assumes the user does not sit down gently. Reports are raised per model, not per range.
The surface you will actually live with
Buyers ask about gloss and colour; the number that matters in service is how the finish stands up to cleaning agents, which is a packing-hall question as much as a spray-booth one.
This stock moves in volume and it is metered at packing as well as at the kiln, because a container of restaurant seating sits in a humid port before it is unloaded, and the reading at destination is the one that matters.
Seats delaminating under daily wiping, stretchers loosening on models that get dragged rather than lifted, and finishes going dull where the cleaning agent is too alkaline. Ask what cleaner the operator uses.
Reference
Questions
What sheen levels can I order?
Matt, satin and semi-gloss on restaurant chairs, all matched to a sealed panel rather than a photo.
Can you match a colour I send?
Physical samples, yes; screen colours, no. Colour is signed off on a stained panel before the batch runs.
How do you keep 300 restaurant chairs the same colour?
One stain batch per order, one reference panel, and the booth checks against it - not against the previous chair.
What finishes are available?
NC, PU and water-based systems; the trade-offs are on the finishing page for restaurant chairs.