Guangdong Chair Factory Notes Production floor, Longjiang · Foshan

Factory Notes › Restaurant Chairs

Machining Tolerances on Restaurant Chairs: Where the Millimetre Is Decided

Tenons, holes and rails on a restaurant chair are held to tenths of a millimetre - the checkpoints that keep a frame square for its whole service life.

Updated 2026-11-09Longjiang, Foshan11 min read

Tenons, holes and rails on a restaurant chair are held to tenths of a millimetre - the checkpoints that keep a frame square for its whole service life.

These notes come off the production floor in Longjiang, Foshan. The current restaurant chairs supplier range is on the main site, with a specification page for every model in it.

Tolerances are set at machining, nowhere else

A restaurant chair frame either leaves the machine shop right or it never comes right. Glue can fill a visible gap but it cannot restore strength, so the millimetre is decided here - at the tenoner, the spindle moulder and the drill press.

Contract frames are machined heavier: legs at 45 to 55 mm, rails at 25 to 30 mm, and a stretcher mortised in on the models that get dragged rather than lifted. That stretcher joint decides whether the chair survives a year of being pulled across a floor.

Joint geometry before joint strength

The tenon is cut a hair proud and the mortise a hair tight, so assembly compresses the fibres and the joint locks itself. The fit is proven against a retained sample before the batch runs.

Corner blocks glued and screwed, stretchers on the heavier models, and a seat rail section big enough to take a repeated racking load. The test regime cycles the frame far harder than a domestic standard does.

A restaurant chair is specified for turnover, not for comfort in the abstract. It gets sat in hard, dragged across a floor and wiped down several times a day. Frames are built to EN 16139 Level 2 and the seat is designed to survive cleaning, which rules out a lot of domestic construction.

FeatureToleranceHow it is checked
Tenon width±0.2 mmGauge every 10th blank
Mortise depth±0.3 mmDepth stop verified at set-up
Hole spacing±0.5 mmDrill jig + plug gauge
Seat rail length±0.5 mmStop block, verified per batch
Surface flatnessRaking lightBefore finishing

Machining checkpoints

Checking without stopping the line

One in ten restaurant chairs blanks goes over the bench during the run: gauge the tenon width, seat depth and hole spacing. If two in a row drift, the cutter gets re-sharpened before anything else moves.

Contract sections run heavier than domestic: 45 to 55 mm legs, 25 to 30 mm rails, and a stretcher on the models that get dragged rather than lifted. The extra section is not for show — it is what survives a room being re-set several times a day.

Wood is still moving after machining

Kiln-dried timber is not finished moving. Boards are allowed to equalise in the workshop before cutting, and machined parts are joined within days, not weeks, so the frame and the environment agree on a moisture number.

Contract sections are thick, and with 490 models this category is most of what goes through the kiln. Thick stock dries slowly and checks if pushed, so the charge is grouped by section and the schedule is written to the thickest blank in it.

A restaurant runs a humid kitchen and an air-conditioned dining room, often in the same building, and the seating sits at whatever the room dictates. Contract frames are therefore built on a joint that tolerates movement rather than one that resists it.

Where tolerance mistakes show up later

Not on day one. They show up as a creaking restaurant chair in year two, which is why the retained sample and the gauge routine exist.

Seats delaminating under daily wiping, stretchers loosening on models that get dragged rather than lifted, and finishes going dull where the cleaning agent is too alkaline. Ask what cleaner the operator uses.

Questions

What tolerance do you hold?

Joint-critical features are held to ±0.2-0.5 mm depending on the feature; the numbers are on the specification sheet for each restaurant chair model.

Why does glue not fix a loose joint?

Glue has strength but no stiffness at the surface - a filled joint flexes, works loose and fails long before the wood does.

Do you check every piece?

One in ten during the run plus a first-article check at set-up; the gauge card travels with the batch.

Can I specify tighter tolerances?

Yes, and it is priced in machine time. Tell us which dimension matters for the installation and we will hold it.