Guangdong Chair Factory Notes Production floor, Longjiang · Foshan

Factory Notes › Restaurant Chairs

Glue, Clamp Time and Corner Blocks on Restaurant Chairs

Moisture, spread, open time and clamp pressure - the four controls that turn glue from a bottle into a process on restaurant chairs.

Updated 2026-10-18Longjiang, Foshan11 min read

Moisture, spread, open time and clamp pressure - the four controls that turn glue from a bottle into a process on restaurant chairs.

These notes come off the production floor in Longjiang, Foshan. The current wholesale restaurant chairs range is on the main site, with a specification page for every model in it.

Glue is a process, not a bottle

The adhesive matters less than the four things around it: moisture of the timber, spread rate, open time and clamp pressure. On a restaurant chair line those four are written down and checked, because they are the difference between a glue line and a glue film.

Stackable models are assembled to a tighter squareness tolerance than a domestic chair, because a stack of six that does not sit true puts a permanent twist into the frames at the bottom. The jig is checked per run, not per season.

Clamp time is not negotiable

Parts come off the clamp bench on a timer, not on feel. A restaurant chair frame unclamped early holds its shape for a day and walks for a year - the rail drifts out of square and the seat deck never sits flat again.

Contract sections are thick, and with 490 models this category is most of what goes through the kiln. Thick stock dries slowly and checks if pushed, so the charge is grouped by section and the schedule is written to the thickest blank in it.

Control pointTargetVerification
Timber moisture8-12%Meter per batch, on the packing list
Spread rateWritten per jointBench check at set-up
Open timeSeason-adjustedTimer on the bench
Clamp pressureSpecified per fixtureRegulator + gauge
UnclampOn timerInspector releases the rack

Glue process control

Corner blocks do the quiet work

Every rail junction gets a glued corner block screwed both directions. They are invisible in the catalogue photos and they are why a frame survives being dragged across a restaurant floor sideways.

A restaurant chair is specified for turnover, not for comfort in the abstract. It gets sat in hard, dragged across a floor and wiped down several times a day. Frames are built to EN 16139 Level 2 and the seat is designed to survive cleaning, which rules out a lot of domestic construction.

Season and shop humidity

Winter glue batches run in drier shops and summer runs in humid ones; open time and cure change with both. The workshop adjusts the spread and the clamp schedule with the season instead of pretending it does not matter.

A restaurant runs a humid kitchen and an air-conditioned dining room, often in the same building, and the seating sits at whatever the room dictates. Contract frames are therefore built on a joint that tolerates movement rather than one that resists it.

What the inspector looks for

Squeeze-out the width of a thread, uniform, and gone after sanding. Heavy squeeze-out means too much spread; none means a dry joint.

EN 16139 Level 2 is the contract grade: higher cycle counts on seat and back, a leg forward load, and a stability test that assumes the user does not sit down gently. Reports are raised per model, not per range.

Seats delaminating under daily wiping, stretchers loosening on models that get dragged rather than lifted, and finishes going dull where the cleaning agent is too alkaline. Ask what cleaner the operator uses.

Questions

What glue do you use?

A D4-class PVA for interior service, and a structural adhesive where the design asks for it; the choice is written into the specification of each restaurant chair.

Is glue harmful after curing?

Cured PVA is inert; our finishes carry the emission documentation buyers usually ask for on restaurant chairs projects.

Why did a joint on my sample open?

Nine times out of ten the timber was too wet at assembly, which is why every batch ships with the moisture record.

Can you glue and screw everything?

We glue structural joints and reserve screws for serviceable parts; all-glued frames are harder to repair and all-screwed frames creep.